Evaluación del efecto de altas temperaturas en la resistencia a compresión y flexión de un hormigón polimérico

Para citar o enlazar este item, por favor use el siguiente identificador: http://dspace.ups.edu.ec/handle/123456789/21516
Registro completo de metadatos
Campo DC Valor Lengua/Idioma
dc.contributor.advisorAndrade Sandoval, Doris Alexandra-
dc.contributor.authorToscano Revelo, Jefferson Daniel-
dc.date.accessioned2021-12-17T15:12:16Z-
dc.date.available2021-12-17T15:12:16Z-
dc.date.issued2021-12-
dc.identifier.urihttp://dspace.ups.edu.ec/handle/123456789/21516-
dc.descriptionEste documento presenta resultados experimentales del efecto de la temperatura en las resistencias a compresión y flexión de un hormigón polimérico, utilizando una resina de poliéster. Para el diseño del hormigón polimérico se tomó como referencia el método de la Densidad Óptima, permitiendo que los vacíos sean ocupados en su totalidad por los agregados pétreos originarios de la cantera de Pifo y en tanto que la resina de poliéster sirvió como ligante para unión de los mismos. Las probetas luego de su curado al ambiente durante 7 días, fueron expuestas en un horno a gas durante 30 minutos y 1 hora, con un aumento constante de 4°C/min hasta alcanzar 100°C, 150°C, 200°C y 250°C. Después de ser ensayadas se observa que la resistencia a compresión y flexión están afectadas directamente por la temperatura y el tiempo de exposición, viéndose perjudicadas a temperaturas mayores a 200°C; para los ensayos a compresión se obtuvo un valor máximo de 84 MPa, en tanto que para las probetas a flexión se consiguió una resistencia máxima de 27 MPa.spa
dc.description.abstractThis paper presents experimental results of the effect of temperature on the compressive and flexural strengths of a polymer concrete, using a polyester resin. For the design of the polymer concrete, the Optimum Density method was used as a reference, allowing the voids to be completely filled by the stone aggregates from the Pifo quarry, while the polyester resin served as a binder to bind them together. The specimens, after curing in the environment for 7 days, were exposed in a gas oven for 30 minutes and 1 hour, with a constant increase of 4°C/min until they reached 100°C, 150°C, 200°C and 250°C. After being tested, it is observed that the compressive and flexural strength are directly affected by temperature and exposure time, being impaired at temperatures higher than 200°C; for the compression tests a maximum value of 84 MPa was obtained, while for the flexural specimens a maximum strength of 27 MPa was achieved.spa
dc.language.isospaspa
dc.rightsopenAccessspa
dc.rightsAtribución-NoComercial-SinDerivadas 3.0 Ecuador*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/3.0/ec/*
dc.subjectINGENIERÍA CIVILspa
dc.subjectEVALUACIÓN DE TECNOLOGÍAspa
dc.subjectRESISTENCIA DE MATERIALESspa
dc.subjectCOMPACTACIÓNspa
dc.subjectFLEXIBILIDADspa
dc.subjectHORMIGÓN POLÍMEROspa
dc.titleEvaluación del efecto de altas temperaturas en la resistencia a compresión y flexión de un hormigón poliméricospa
dc.typebachelorThesisspa
ups.carreraIngeniería Civilspa
ups.sedeSede Quitospa
Pertenece a las colecciones: Grado

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
UPS - TTS570.pdfTexto completo640,53 kBAdobe PDFVisualizar/Abrir


Este ítem está sujeto a una licencia Creative Commons Licencia Creative Commons Creative Commons